Home Categories Send inquiry

Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer

Available Products

Seamless tube, Plate, Rod, Forgings, Fasteners, Pipe Fittings

Production Standards

Product

ASTM

Bar

B 446

Plate, Sheet and Strip

B 443, B 906

Seamless pipe,tube

B 444, B 829

Welded pipe

B 705, B 775

Welded fittings

B 704, B 751

Welded connectors

B 366

Forged billets and bars

B 472

Forging

B 564

Chemical Composition

%

Ni

Cr

Mo

Fe

C

Mn

Si

P

S

Co

Nb+Ta

Al

Ti

Min

58.0

20.0

8.0

3.15

Max

23.0

10.0

5.0

0.10

0.50

0.50

0.015

0.015

1.00

4.15

0.40

0.40

Physical Properties

Density

8.36 g/cm3

Melting

1330-1375℃

Inconel 625 Features

1. Excellent corrosion resistance to various corrosive media in oxidizing and reducing environments
2. Excellent resistance to pitting corrosion and crevice corrosion, and will not produce chloride ion stress corrosion cracking
3. Excellent corrosion resistance to inorganic acids, such as nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid and mixed acids of sulfuric acid and hydrochloric acid, etc.
4. Excellent resistance to corrosion of various inorganic acid mixed solutions
5. When the temperature reaches 40℃, it can show good corrosion resistance in various concentrations of hydrochloric acid solution
6. Good workability and weldability, no post-weld cracking sensitivity
7. Manufacture certification of pressure vessels with wall temperature of -196~450℃
8. Certified by the American Society of Corrosion Engineers NACE standard (MR-01-75) to meet the highest standard level VII for use in sour gas environments.

Inconel625 Application Areas

The softened and annealed low carbon alloy 625 is widely used in the chemical process industry, and its better corrosion resistance and high strength enable it to be used as a thinner structural component. Alloy 625 can be used in applications exposed to seawater and subject to high mechanical stress. Typical application areas:
1. Components of organic chemical processes containing chlorides, especially where acid chloride catalysts are used
2. Digesters and bleaching tanks for the pulp and paper industry
3. Absorption tower, reheater, flue gas inlet baffle, fan (humid), agitator, deflector and flue in flue gas desulfurization system
4. For the manufacture of equipment and components for use in sour gas environments
5. Acetic acid and acetic anhydride reaction generator
6. Sulfuric acid condenser


Superalloy Inconel625/ UNS N06625/ Alloy625 Manufacturer Related Video: